Shrinkage Reduction Type High-Strength Concrete using Waste Roof Tile
This is low shrinkage type high-strength concrete with self-shrinkage reduction property, which is produced by mixing the absorbed waste roof tile into the concrete and supplying water from inside of concrete. Simultaneously, self-shrinking cracks, which usually occurred in high-strength concrete can be suppressed.
- Specifications
-
- 1Design Standard Strength: About 100N/mm2
- 2Slump Flow: 675±75mm